Crocking and perspiration fastness are the two tests that most often sink a garment trims lot: a dyed woven label, printed care label, webbing or elastic that bleeds costs the whole shipment, and the blame usually lands on a trims supplier that never ran the dye bath. This guide covers how each test is run, how to read the grade, the four real causes of failure, and how to fix a lot without changing its colour.

1. What each test actually measures

The crocking test rubs a dry and a wet white cotton square against the specimen and grades the staining of that white cloth; the perspiration test sandwiches the specimen against multi-fibre control fabric, soaks it in artificial perspiration, then presses and heats it, grading staining in acid and alkaline solution separately. Crocking predicts transit and shop-floor abrasion; perspiration predicts skin contact — neck labels, care labels and hem tape. Both grade staining, not colour change, which is where most disputes start: your swatch kept its shade while the buyer's white control cloth turned pink.

2. Methods, conditions and typical limits

Test Method and condition Typical limit
Dry crocking ISO 105-X12 or AATCC 8, 9 N load, 10 strokes 4 or above
Wet crocking Same method, white cloth at about 100 % pick-up 3 or above; deep shades 3–4
Acid perspiration ISO 105-E04 or AATCC 15, pH 5.5, 37 °C, 4 hours 4 or above; childrenswear 4–5
Alkaline perspiration ISO 105-E04, pH 8.0, 37 °C, 4 hours 4 or above

3. How to read the grade, and the three things to check on the report

Staining is graded 1–5 against the grey scale with half grades allowed; 4 and above is normally treated as commercially acceptable. Read three things on the report: whether it graded staining or colour change, whether dry and wet are reported separately, and whether the control cloth was single-fibre cotton or multi-fibre. A report that states one number, grade 4, cannot settle a dispute or tell a dye problem from an ink problem. Make sure the lot number on the report matches the bulk, and re-test after any dye-bath or ink-batch change.

4. Four real causes of a failure

  • Dye class: sulphur or direct dyes on deep-coloured cotton labels are cheap but inherently weak in wet crocking; a reactive dye usually buys a full grade
  • Weak fixation: shortened soaping and under-dosed fixing agent pass at the factory and bleed after one wash
  • Ink and binder: dark screen ink over a light base, incompletely cured, or a binder with poor water resistance fails wet crocking first
  • Softener and silicone residue: hand-feel improves while crocking drops half a grade to a full grade — a softener added for touch is the usual hidden culprit

5. Set limits by end use, not one number for everything

The same webbing specified for babywear and for outerwear sits a full grade apart. For next-to-skin baby pieces (0–3 years) ask for 4–5 in dry and wet crocking and acid perspiration; underwear and activewear 4; denim and exposed tape 4 dry and 3 wet; decorative non-contact care labels can relax to 3–4. Put those numbers in the trim specification sheet rather than arguing over a report later: the cost difference is usually a few yuan per thousand pieces, far below one return shipment.

6. How to fix a failing lot without changing its colour

Fix the process, not the hue: longer soaping and hot rinsing, a full dose of cationic fixing agent, sulphur dye replaced by a reactive in the same shade range, ink switched to UV or given a crosslinker, silicone softener replaced with a hydrophilic one. Re-test and re-issue under a new lot number; the old report cannot be carried over, because the first thing a customer checks is lot number against test date. If the shade was specially approved, send 0.5 m of tape or 50 pieces for shade confirmation before touching the bulk.

7. The label still has to be legally right while you fix the lot

Fastness is a market-access question, but label content is a legal precondition, and the two do not mix. In the EU, fibre composition follows (EU) No 1007/2011 and care symbols follow the EN ISO 3758 system; France adds the mandatory mentions of the Code de la consommation, Germany the Textilkennzeichnungsgesetz, Spain Real Decreto 928/1987 with fibre content and a reference number. Japan requires fibre blend ratio and care labelling under the Household Goods Quality Labelling Act with the JIS L 0001 symbol set, and Korea requires blend ratio and handling precautions under the Quality Management and Safety Control of Industrial Products Act. Once a claim on the label contradicts a test result, the fix becomes a relabelling job with double the cost and risk.

8. Pre-shipment checklist

  • Report lot matches the goods and the test date is within 12 months
  • Dry and wet reported separately, staining and colour change graded separately
  • Keep three retention samples of every deep shade for the buyer's own retest
  • Label content does not contradict the test conclusions: fibre, care, origin
Fastness is made, not tested. Discovering grade 2–3 wet crocking after the report means either re-dyeing the lot or gambling that the buyer will not retest. Put the limits in the specification and run one test at sampling stage: the cost is a few samples, the payoff is a shipment that does not come back.