Pocketing is the panel most often trimmed out of a cost sheet and the first one to wear through. It rubs against whatever is in the pocket, gets pushed in and out by a hand all day, and goes through every wash and dry the garment does. Holes, pilling and colour bleeding into the lining almost always start here. Choosing pocketing does not need a hand-feel argument: four numbers settle it, weight, shrinkage, crocking fastness and perspiration fastness, plus the chemical limits of each destination market.

1. Five Pocketing Fabrics, Five Jobs

Polyester taffeta, 190T or 210T at 55 to 75 g/m², is the workhorse for trousers and outerwear: thin, slick, cheap, low drag on the hand, but prone to static and snagging. Cotton poplin at 110 to 130 g/m² breathes and feels good against skin, which suits shirts and childrenswear, though it must be pre-shrunk. Denim pocket bags use cotton twill or a knit jersey at 150 to 220 g/m² that has to survive stone washing. Sportswear and underwear take mesh at 80 to 120 g/m² for quick drying and softness. Tailored jackets use cupro or a polyester viscose blend for drape and slip, at the highest cost.

2. Weight and Shrinkage: Get These Two Right First

Taffeta below 55 g/m² wears through at the pocket corners; above 90 g/m² the pocket reads bulky and disturbs the line of the garment. Cotton pocketing should shrink no more than 3 percent warp and 2 percent weft, or the pocket pulls the side seam out after washing. Test it the way buyers ask: one wash at 60 °C and one tumble dry, then measure. If pocketing and shell differ by more than 2 percentage points in shrinkage, the pocket will either peek out or the shell will bunch, and no amount of pressing fixes it.

Pocketing type Weight Best for
Polyester taffeta 190T 55 to 65 g/m² Trousers, chinos, outerwear
Cotton poplin, pre-shrunk 110 to 130 g/m² Shirts, childrenswear, next to skin
Cotton twill 150 to 180 g/m² Denim, workwear
Knit jersey 180 to 220 g/m² Denim, stretch trousers
Mesh 80 to 120 g/m² Sportswear, underwear, swim

3. Colorfastness: The Side That Rubs Against Skin

The demands on pocketing are routinely underestimated. A dark pocket bag that bleeds onto a pale lining or shell is one of the most common claims a garment factory faces. Three test items settle it: crocking fastness at grade 4 or better dry and grade 3 or better wet; perspiration fastness, acidic and alkaline, at grade 3 to 4 or better; and wash fastness at 40 °C for five cycles with colour change at grade 4 and staining at grade 3 to 4. Navy, black and deep red are the three colours that fail most, so test at sampling, not at final inspection.

4. Chemical Limits: Every Market Draws a Different Line

China s GB 18401 class B, for direct skin contact, caps formaldehyde at 75 mg/kg, requires pH between 4.0 and 8.5, and bans cleavable aromatic amine dyes. In the EU, REACH limits azo dyes to 30 mg/kg and requires notification above 0.1 percent for SVHCs. In the United States, children s products fall under CPSIA while adult apparel relies on buyer restricted substance lists. Japan requires fibre composition and care labelling under the Household Goods Quality Labelling Act, with hazardous substances governed separately. Korea requires fibre content and care instructions, plus KC safety confirmation for children s products. One lot of pocketing shipped to three markets needs three test reports.

5. Purchase Order and Inspection List

  • Fix fibre and weight: 100 percent polyester at 65 g/m² plus or minus 3 percent, not just polyester fabric
  • State width and usable width separately, for example 150 cm width with 148 cm usable
  • Shrinkage and the test method: one wash at 60 °C and one tumble dry
  • The three fastness grades plus colour difference within Delta E 1.0 across dye lots
  • A test report per lot covering formaldehyde, azo dyes and pH, with lot number matching the roll label
Four numbers: 65 g/m² within 3 percent, shrinkage at or below 3 percent, dry crocking at grade 4, formaldehyde at or below 75 mg/kg. Put all four on the purchase order and the pocketing is actually specified.

Pocketing usually accounts for 1 to 2 percent of a garment bill of materials, yet it decides whether a pocket lasts two years, whether the bag peeks out after washing, and whether a dark colour ruins the lining. Fix the four items, weight, shrinkage, fastness and chemical limits, and purchasing and the garment factory judge to the same standard. What you save is not the 1 percent of fabric cost but the labour hours that go into claims and rework.

Related Articles

Sourcing pocketing? Send the application, weight, colour and destination markets and we will return a specification with shrinkage and fastness test conditions, matching chemical limits, plus a same-dye-lot swatch.

Request a pocketing spec →